51 31... Instructions on gluing windshield: Notes
WARNING: This page does not describe the selected car, but rather 7 other vehicles, including the 2003 BMW 540i, 2002 BMW 540i, 2001 BMW 540i, 2000 BMW 540i, and 1999 BMW 540i. However, it is still accessible from the selected car via links, so may be relevant.
IMPORTANT:
Storage temperature of all adhesive products of 5°C to 25°C must be observed.
Special instructions for hot processing must be observed:
Special instructions for hot processing must be observed:
- Temperature of cartridge oven must be checked every morning with DIS or GT1
- Temperature of cartridge < 80°C results in the formation of bubbles/blisters (gluing/cementing not permitted)
- Insufficient heating (< 1 hour) results in the formation of bubbles/blisters (gluing/cementing not permitted)
- Heating time or a cartridge max. 8 hours
- Mistake in mixing in event of an interruption in application >1 minute (gluing/cementing not permitted)
- A test bead of 50..70 mm must be rejected after an interruption in application
- Cartridge may only be heated up once; if the lower label is black, this adhesive may only still be used cold without accelerator while adhering to the Best before date.
These instructions are not applicable to door window cementing (door "center") on the E38/L7:
Work steps for removing and installing windshields:
- is displayed at the end of this document by clicking on the "framed cross-reference"